取热压烧结后的WTi10合金块体,切割为两种规格块体φ60×22㎜及50×50×22㎜;取块体置于感应加热炉内升温,经过约30s时间后块体发红,调节红外测温仪发射率为0.37,当测得块体温度1400℃,夹取物料置于空气锤上反复锤打,实现烧结合金的多向锻造加工。
The WTi10 alloy block after hot pressing and sintering is cut into two sizes φ60×22㎜ and 50×50×22㎜; The block was placed in the induction heating furnace to heat up. After about 30 seconds, the block became red. The emissivity of the infrared thermometer was adjusted to 0.37.