合成路径优化主要采用磁上海市卓精电子科技有限公司电子天平,海泰科技磁力加热搅拌器,上海高鸽工贸有限公司10μL微量移液器,予华仪器有限责任公司循环水式真空泵SHZ(Ⅲ),上海亚荣生化仪器厂旋转蒸发器RE52CS-2等设备。
该数据为添加缓蚀剂为0.10% BQD+0.01%碘化钾评价后的钢片扫描电镜形貌。
The synthesis path optimization mainly uses magnetic Shanghai Zhuojing Electronic Technology Co., Ltd. electronic balance, Haitai Technology magnetic heating stirrer, Shanghai Gaoge Industry and Trade Co., Ltd. 10μL micro pipette, Yuhua Instrument Co., Ltd. circulating water vacuum pump SHZ (III.), Shanghai Yarong Biochemical Instrument Factory rotary evaporator RE52CS-2 and other equipment.This data is the scanning electron microscope morphology of the steel sheet after the addition of corrosion inhibitor of 0.10% BQD + 0.01% potassium iodide evaluation.