制备所得的高比重钨合金路亚拟饵成分比为钨:镍:铁=(8.0~9.7):(1.0~0.25):(1.0~0.05),制备方法的具体步骤:一、将钨粉、镍粉和铁粉按设计好的配比进行称重、混合得到均匀的合金粉末;二、将体积比为(2.8~4.1):(7.2~5.9)的合金粉末和成型剂密炼得到喂料;三、将喂料进行破碎得到喂料颗粒;四、将喂料颗粒注射成型得到注射生坯;五、将注射生坯溶剂脱脂得到溶剂脱脂坯;六、将溶剂脱脂坯热脱脂得到热脱脂坯;九、将热脱脂坯氢气保护烧结得到高比重钨合金路亚拟饵。制备的高比重钨合金路亚拟饵为一体式的,环保的,且具有高的强度。
The composition ratio of tungsten: nickel: iron = (8.0~9.7): (1.0~0.25): (1.0~0.05) of the prepared high specific gravity tungsten alloy lure, the specific steps of the preparation method: a. weigh and mix tungsten powder, nickel powder and iron powder according to the designed ratio to obtain uniform alloy powder; b. mix the volume ratio of (2.8~4.1): (7.2~5.9) The alloy powder and the forming agent are densely refined to obtain the feed material; iii. The feed material is crushed to obtain the feed material particles; iv. The feed material particles are injected to obtain the injection billet; v. The injection billet is solvent degreased to obtain the solvent degreased billet; vi. The solvent degreased billet is hot degreased to obtain the hot degreased billet; i. The hot degreased billet is hydrogen-protected sintered to obtain the high specific gravity tungsten alloy lure. The prepared high specific gravity tungsten alloy roadkill lure is one-piece, environmentally friendly, and has high strength.