Cu-Ni-Co-Si合金(PW47100)带材抗拉强度为892MPa,屈服强度为862MPa,抗软化温度524℃,导电率46.8%IACS
有色院提供报告仅提供抗拉强度,屈服强度数值,未提供应力应变曲线抗软化实验过程在附件中。
The tensile strength of Cu Ni Co Si alloy (PW47100) strip is 892MPa, the yield strength is 862MPa, the softening temperature is 524 ℃, and the conductivity is 46.8% IACS