GH984G不同磷含量锻态合金的真应力-应变曲线 (a) 950 °C / 0.01 s-1,(b) 950 °C / 1.0 s-1,(c) 1150 °C / 0.01 s-1,(d) 1150 °C / 1.0 s-1
The true stress-true strain curves of forged alloys after deformation at 950 °C / 0.01 s-1 (a), 950 °C / 1.0 s-1 (b), 1150 °C / 0.01 s-1 (c) and 1150 °C / 1.0 s-1 (d).