EH40钢在添加不同浓度锌离子的海水中浸泡不同时间的去除腐蚀产物的表面CLSM图片及对应最大蚀坑深度截面轮廓图(A-C:分别为浸泡1周、2周、4周;1-3:分别为添加0 mmol·L-1、1.5 mmol·L-1、15 mmol·L-1)
Surface CLSM images and corresponding maximum pit depth section profiles of EH40 steel where corrosion products were removed after being immersed in seawater added different concentrations of zinc ions for different time (A-C: immerse for 1 week, 2 weeks and 4 weeks respectively; 1-3: add 0 mmol·L-1, 1.5 mmol·L-1 and 15 mmol·L-1 respectively)