碱式碳酸锆与氢氧化钠溶液在反应釜分别在110、140、170、200 ℃高温下加热6 h,形成ZrO2晶体结构。并进行氧化锆的拉曼测试
ZrO2 crystal structure was formed by heating basic zirconium carbonate and sodium hydroxide solution at 110, 140, 170 and 200 ℃ for 6 h in a reaction kettle. Raman test of zirconia was carried out.