将碱式碳酸锆与氢氧化钠溶液加入水热反应釜,分别高温加热6 、12、24、36、48h,形成ZrO2晶体结构。测试其XRD谱图
Add basic zirconium carbonate and sodium hydroxide solution to a hydrothermal reaction kettle. ZrO2 crystal structure was formed by heating at high temperature for 6, 12, 24, 36 and 48h respectively. Then their XRD pattern were tested