将碱式碳酸锆与制备的氢氧化钠溶液一起转入水热反应器。反应釜分别在室温、100、300、500℃下加热6 h,形成ZrO2晶体结构。测试其XRD谱图
The basic zirconium carbonate and the prepared sodium hydroxide solution are transferred to a hydrothermal reactor. The reaction kettle was heated at room temperature, 100, 300 and 500℃ for 6 h to form ZrO2 crystal structure. Its XRD pattern was tested