将碱式碳酸锆与制备的氢氧化钠溶液一起转入水热反应器。反应釜分别在110、140、170、200℃高温下加热6 h,形成ZrO2晶体结构。测试其XRD谱图
The basic zirconium carbonate and the prepared sodium hydroxide solution are transferred to a hydrothermal reactor. The reaction kettle was heated at 110, 140, 170 and 200 ℃ for 6 h to form the crystal structure of ZrO2. Then its XRD pattern was tested