不同碳热还原制度下,(HfNbTaTiW)C预固溶粉X射线图谱,(HfNbTaTiW)C预固溶粉X射线图谱中FCC1与FCC2相在第一组晶面族{100}处的衍射峰强比
X-ray diffraction patterns of (HfNbTaTiW)C powders obtained through CTR at 1400–1800℃;the relative intensity PFCC2/PFCC1 of the first set ({100}) of peaks corresponding to FCC1 and FCC2 phases of (HfNbTaTiW)C powders obtained through CTR at 1400–1800 ℃